S275N steel is carbon and low alloy steel under the standard EN10113. EN10113 S275N means when the temperature is not less than -20℃, the minimum impact values is required. The delivery condition for S275N steel is normalizing rolling.
S275N steel chemical composition:
Grade | Thk mm |
Delivery condition | Chemical composition % | ||||||||
C | Si | Mn | P | S | Ni | TA1 | Nb | Ceq | |||
S275N | standard | ≤0.18 | ≤0.40 | 0.50-1.40 | ≤0.035 | ≤0.030 | ≤0.50 | ≥0.020 | ≤0.050 | Same as below | |
8 | normalizing | 0.14 | 0.2 | 0.9 | 0.02 | 0.18 | 0.15 | 0.02 | 0.015 | ≤0.40 | |
T>100 | 0.18 | 0.4 | 1.1 | 0.25 | 0.04 | 0.03 | ≤0.42 |
S275N steel processing properties: Cold cracks may occur as the thickness and strength level higher. Cold crack is integrated by the following factors: 1, The amount of diffusion hydrogen in the welding metal. 2, The brittleness of heat affected zone 3, The tensile stress concentration at welding joint. S275N normalized steel mechanical properties at room temperature:
Grade | minimum Yield strength ReH,Mpa N/mm2 |
|||||||
Thickness, mm | ||||||||
≤16 | >16-40 | >40-63 | >63-80 | >80-100 | >100-150 | >150-200 | >200-250 | |
S275N | 275 | 265 | 255 | 245 | 235 | 225 | 215 | 205 |
Grade | Tensile strength N/mm2 MPa | The minimum elongation after fracture L0=5.65√S0 |
|||||||
Thickness, mm | Thickness, mm | ||||||||
≤100 | >100-200 | >200-250 | ≤16 | >16-40 | >40-63 | >63-80 | >80-200 | >200-250 | |
S275N | 370-510 | 350-480 | 350-480 | 24 | 24 | 24 | 23 | 23 | 23 |